Semiconductor inspection / technical guide

SWIR Imaging for
Wafer Bonding Inspection.

Seeing through silicon to examine bonding interfaces, alignment features and selected hidden defects.

THROUGH-SILICON IMAGINGINGAAS SWIRWAFER BONDINGNON-DESTRUCTIVE INSPECTION

In advanced semiconductor manufacturing, some of the most consequential defects are not on the wafer surface. Voids, misaligned features and imperfections at bonded interfaces can remain hidden beneath silicon, where conventional visible-light cameras cannot directly inspect them.

Short-wave infrared (SWIR) imaging provides a non-destructive way to investigate selected subsurface structures. With the right wavelength, illumination and optics, an InGaAs camera can capture features through silicon and help engineers evaluate bonded wafers, MEMS devices and advanced packaging assemblies.

This guide explains how SWIR wafer bonding inspection works, which defects it may reveal, and how to select suitable cameras from the Rapixel SWIR camera portfolio.

01 / Inspection challenges

What Makes Wafer Bonding Inspection Difficult?

Wafer-to-wafer and die-to-wafer bonding join multiple layers into a single structure. Inspection after bonding is difficult because relevant features may no longer be accessible from the visible surface.

01

Bond Voids & Incomplete Contact

Unbonded regions, trapped gas or interface gaps may affect the integrity of selected bonded structures.

02

Alignment & Registration

Buried alignment marks, seal rings and die features may need to be located through a silicon layer.

03

Subsurface Cracks

Cracks introduced during handling, thinning or dicing may extend below the visible surface.

04

Advanced Packaging Structures

Stacked devices, MEMS cavities and selected die-attach interfaces can require imaging from an accessible side.

02 / Imaging principle

Why Can SWIR Cameras See Through Silicon?

Silicon strongly absorbs much of the visible spectrum. Its transmission generally increases at wavelengths beyond its band-edge region near 1.1 μm, although actual transmission depends on wafer thickness, doping, surface condition, temperature and the complete optical path.

InGaAs SWIR cameras are sensitive to wavelengths commonly used for through-silicon imaging. When illuminated appropriately, features such as alignment marks, interfaces, cracks or some voids may create measurable differences in transmitted or reflected intensity.

Important: “Seeing through silicon” does not mean seeing through every semiconductor stack. Metal films, opaque coatings, heavily absorbing layers and some packaging materials can block the optical path. SWIR also cannot guarantee detection of every bond void.

For a practical starting point, engineers often evaluate illumination in the approximately 1100–1550 nm region, then adjust wavelength according to silicon thickness, stack materials and defect contrast. This is a system-design range, not a universal optimum for all wafers.

03 / Optical setup

Transmission vs. Reflection: Choose the Right Geometry

Transmission SWIR Imaging

The light source and camera sit on opposite sides of the sample. Light passes through the wafer stack, and interfaces or defects alter the transmitted signal. This can be effective for inspecting bonded pairs when both sides are accessible.

Reflection SWIR Imaging

The illumination and camera operate from the same accessible side. Light travels into silicon and returns from an internal interface or reflective feature. This can help when backside access is limited, but contrast and interpretation are more demanding.

What changes between the two approaches?

  • Access: transmission normally requires both sides of the wafer; reflection can work from one side.
  • Contrast: transmission often provides more straightforward shadow or attenuation contrast for some buried features.
  • Material stack: metal and other opaque layers can prevent useful imaging in either geometry.
  • Validation: flat-field correction, optical baffling, focus and representative samples are essential.
04 / Target applications

Where Does SWIR Add Value in Wafer Bonding?

APPLICATION A

Bond Interface & Void Examination

Evaluate selected unbonded areas, interface irregularities or cavity features in silicon-based wafer stacks under suitable transmitted or reflected illumination.

APPLICATION B

Through-Silicon Alignment

Locate buried alignment marks or seal-ring structures when assembling wafers or monitoring registration in MEMS and advanced packaging workflows.

APPLICATION C

Wafer Cracks & Edge Damage

Examine subsurface damage associated with cutting, grinding or wafer handling when contrast is sufficient in the selected optical setup.

APPLICATION D

Die & Package R&D

Investigate optically accessible internal features in research and failure-analysis environments without immediately resorting to destructive sectioning.

These are potential imaging applications, not a claim that every camera detects every defect type or that a particular defect-size threshold has been validated.

05 / Rapixel camera options

Recommended Rapixel SWIR Cameras for Wafer Inspection

The best camera depends on sampling requirements, inspection geometry, stage motion and wavelength. The following models provide different integration choices for through-silicon inspection development.

High-Resolution Wafer Imaging — iBoostX IMX992 (5.2 MP)

For systems that need detailed imaging across a relatively large field of view, the Rapixel iBoostX IMX992 SWIR camera offers 2560 × 2048 pixels, a specified 400–1700 nm spectral range, and multiple interface variants. The listed maximum 165 fps applies to a specific 10GigE configuration; other interfaces have different rates. Higher pixel count can support finer spatial sampling, provided the optics and contrast are sufficient.

Fast Area Inspection — iBoostX IMX993 (3.1 MP)

The Rapixel iBoostX IMX993 combines 2048 × 1536 resolution with up to 150 fps, a 400–1700 nm response, Camera Link and built-in TEC cooling. It is worth evaluating for inspection stations requiring high acquisition rates and thermal stability.

Flexible Development Platform — iBoostX IMX990 (1.3 MP)

For laboratory setups, prototype tools and integrated inspection stations, the Rapixel iBoostX IMX990 provides 1280 × 1024 resolution with USB 3.0 or GigE variants, specified up to 200 fps on USB 3.0. Its product page lists a 400–1800 nm spectral range; sensor response at a chosen wavelength should be confirmed for the actual variant.

Extended-Wavelength Evaluation — iBX-SWU640B

The Rapixel iBX-SWU640B offers 640 × 512 imaging with variant-dependent coverage of 1000–1900 nm or 1200–2200 nm. It can be considered when testing longer SWIR wavelengths for demanding silicon stacks or materials research, after checking illumination, optical transmission and signal levels.

Continuous Scanning Architecture — iBoost40GSW2KM

For systems built around controlled wafer-stage motion, the Rapixel iBoost40GSW2KM SWIR line scan camera provides 2048 × 1 pixels, a specified 40 kHz line rate, 950–1700 nm sensitivity and GigE connectivity. A line scan architecture may be suitable for building continuous images of moving substrates when illumination and synchronization are correctly engineered.

Camera Resolution Spectral range Acquisition Consider for
iBoostX IMX992 2560 × 2048 400–1700 nm Up to 165 fps* High-resolution area imaging
iBoostX IMX993 2048 × 1536 400–1700 nm Up to 150 fps Fast inspection stations
iBoostX IMX990 1280 × 1024 400–1800 nm Up to 200 fps* R&D and prototyping
iBX-SWU640B 640 × 512 1000–1900 / 1200–2200 nm* 240 / 270 fps* Longer-wavelength evaluation
iBoost40GSW2KM 2048 × 1 950–1700 nm 40 kHz line rate Continuous wafer scanning

*Maximum acquisition rates and spectral ranges depend on the selected model or interface variant. Confirm final configuration and up-to-date specifications before system design.

06 / System selection

How to Design an Effective SWIR Wafer Inspection System

01

Define the structure and defect

Identify the wafer material, stack thickness, bonding process and target defect. A bond void, buried alignment mark and hairline crack may require very different illumination and resolution strategies.

02

Choose the imaging geometry

Determine whether transmission or reflection is physically possible. Map metal layers, opaque coatings and all interfaces between the source and the camera.

03

Select wavelength, illumination and optics

Compare candidate wavelengths using real samples. SWIR-compatible lenses, filters, source uniformity, working distance and optical magnification can matter as much as camera resolution.

04

Calculate spatial sampling

For example, a 100 mm field of view across 2560 horizontal pixels gives about 39 μm per pixel. This is sampling, not a guaranteed minimum detectable void or crack size; optical resolution and defect contrast must also be validated.

05

Validate with known samples

Use reference wafers and documented defects to evaluate contrast, false positives, image uniformity, repeatability and throughput before qualifying the inspection process.

For critical bonding processes: SWIR may complement, rather than replace, established inspection methods such as scanning acoustic microscopy, X-ray or destructive failure analysis. The suitable method depends on defect depth, size and material stack.
07 / Practical FAQ

Frequently Asked Questions

Can SWIR cameras inspect a bonded wafer without cutting it?

Yes, in suitable silicon-based structures, SWIR can support non-destructive imaging of some buried features. The result depends on illumination, thickness, material layers and access geometry.

Which wavelength is best for seeing through silicon?

There is no single optimum wavelength. Approximately 1100–1550 nm is a common evaluation region, while thickness and stack materials may justify testing other wavelengths and checking sensor sensitivity.

Can SWIR detect every wafer-bonding void?

No. Detectability depends on the void's size, orientation, contrast, surrounding materials and imaging configuration. Metallic and strongly absorbing layers can hide features entirely.

Is a 5.2 MP SWIR camera always preferable to a 1.3 MP model?

No. Higher resolution improves sampling at a given field of view, but the best choice also depends on optics, throughput, light levels, data rate, system cost and required defect visibility.

What is the difference between SWIR wafer bonding inspection and UV TDI wafer surface inspection?

SWIR is often evaluated for optically accessible subsurface structures and bonding interfaces through silicon. UV TDI is evaluated for selected fine surface features during high-resolution scanning. They address different inspection needs.

08 / Semiconductor knowledge hub

Explore Related Imaging Technologies

Connect wafer-bonding inspection with complementary surface imaging, optical system design and the wider Rapixel camera portfolio.

When your first two Semiconductor Knowledge Hub articles are published, add their exact article URLs here to complete the three-article SEO cluster. Avoid linking to unpublished pages.

09 / Discuss your application

Build a Through-Silicon Imaging System with Rapixel

Developing a wafer bonding inspection or semiconductor failure-analysis system? Share your wafer stack, target defects, field of view, preferred wavelength, inspection speed and interface requirements. The Rapixel team can help you evaluate suitable SWIR camera options.

Explore Rapixel SWIR Cameras

Technical inquiries: info@rapixeltech.com

Technical note: All application descriptions are examples for system evaluation. Detection limits and suitability are not guaranteed without testing with representative samples. Confirm product specifications and options with Rapixel before purchase.

Latest Stories

لا يتضمن هذا القسم حاليًا أي محتوى. يمكنك إضافة محتوى إلى هذا القسم باستخدام الشريط الجانبي.